Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Ceramic > Keyword: silica
8 micrographs available, ordered by micrograph number.
![]() |
Micrograph
150
:
Alumina-zirconia-silica (AZS) refractory brick System: Al2O3-ZrO2-SiO2, Composition: Al2O3 50, ZrO2 32, SiO2 15 (wt%), + trace alkalis Reflected light microscopy 300 μm |
![]() |
Micrograph
155
:
Silica investment casting core System: SiO2, Composition: SiO2, trace of clay Reflected light microscopy 300 μm |
![]() |
Micrograph
172
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
173
:
Bone china, showing the glaze on the surface (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
174
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
542
:
Devitrified Glass: glass sample heated at 900°C for 17 hours. System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
543
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
544
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.