Micrograph
542
:
Devitrified Glass: glass sample heated at 900°C for 17 hours. System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
543
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
544
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
650
:
Small ceramic pot showing centimetre scale crystals within the glaze System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%) Photography (no microscope) 20 mm |
![]() |
Micrograph
655
:
Small ceramic pot showing centimetre scale crystals within the glaze System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%) Photography (no microscope) 5 mm |