Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Ceramic > Keyword: magnesium
3 micrographs available, ordered by micrograph number.
![]() |
Micrograph
148
:
Magnesia-chrome refractory brick System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%) Reflected light microscopy 1 mm |
![]() |
Micrograph
149
:
Magnesia-chrome refractory brick System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
154
:
Macor(TM) Machinable Glass Ceramic System: MAS (MgO-Al2O3-SiO2), Composition: SiO2 47, B2O3 8, Al2O3 17, MgO 14, K2O 9, F 6 (wt%) Reflected light microscopy 20 μm |