Categories > Ceramic > Triaxial (i.e. clay/flux/filler) porcelain
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
190
:
Aluminous Electrical Porcelain System: Triaxial (i.e. clay/flux/filler) porcelain, Composition: Ball clay 30 , china clay 10, potash feldspar 20, silica sand 20, calcined alumina 20 (wt%) Scanning electron microscopy (SEM) 10 μm |