Browse the Library
Categories > Ceramic > ZrO2-Y2O3
3 micrographs available, ordered by micrograph number.
![]() |
Micrograph
196
:
Tetragonal Zirconia Polycrystals (TZP) System: ZrO2-Y2O3, Composition: Y2O3 2-3, ZrO2 96-97 (wt%) Bright-field TEM 600 nm |
![]() |
Micrograph
848
:
Physical vapour deposited (PVD) partially stabilized zirconia (PSZ) showing columnar structure System: ZrO2-Y2O3, Composition: ZrO2 92.5, Y2O3 7.5 (wt%) Field emission gun scanning electron microscopy (FEGSEM) 1 μm |
![]() |
Micrograph
849
:
Partially stabilized zirconia (PSZ) powder for plasma spraying System: ZrO2-Y2O3, Composition: ZrO2 92.5, Y2O3 7.5 (wt%) Scanning electron microscopy (SEM) 100 μm |