Categories > Ceramic > Scanning electron microscopy (SEM)
8 micrographs available, ordered by micrograph number.
![]() |
Micrograph
117
:
Sintered disc of Hydroxyapatite (Ca10(PO4)6(OH)2), a calcium phosphate ceramic with similar composition to natural bone mineral System: Hydroxyapatite (Ca10(PO4)6(OH)2), Composition: Not specified Scanning electron microscopy (SEM) 18 μm |
![]() |
Micrograph
190
:
Aluminous Electrical Porcelain System: Triaxial (i.e. clay/flux/filler) porcelain, Composition: Ball clay 30 , china clay 10, potash feldspar 20, silica sand 20, calcined alumina 20 (wt%) Scanning electron microscopy (SEM) 10 μm |
![]() |
Micrograph
548
:
Fractograph showing extensive matrix cracking and fibres bridging an opened matrix in a fibre reinforced magnesium aluminosilicate ceramic System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Scanning electron microscopy (SEM) 200 μm |
![]() |
Micrograph
564
:
Aligned array of nanotubes System: Carbon nanotube, Composition: Not specified Scanning electron microscopy (SEM) 25 μm |
![]() |
Micrograph
565
:
Vapour-grown carbon nanotubes System: Carbon nanotube, Composition: Not specified Scanning electron microscopy (SEM) 5 μm |
![]() |
Micrograph
594
:
Carbon string System: C, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
![]() |
Micrograph
628
:
Sintered salt (NaCl) System: Na-Cl, Composition: Not specified Scanning electron microscopy (SEM) 140 μm |
![]() |
Micrograph
849
:
Partially stabilized zirconia (PSZ) powder for plasma spraying System: ZrO2-Y2O3, Composition: ZrO2 92.5, Y2O3 7.5 (wt%) Scanning electron microscopy (SEM) 100 μm |