Categories > Ceramic > BaTiO3 Ag/Pd > BaTiO3 > Keyword: silver
1 micrograph available, ordered by micrograph number.
Micrograph
153
:
Barium Titanate Ag/Pd Multilayer Capacitor System: BaTiO3 Ag/Pd, Composition: BaTiO3 Reflected light microscopy 300 μm |