Browse the Library
Categories > Ceramic > LAS: Li2O-Al2O3-SiO2 > Transmitted polarised light microscopy, with sensitive tint plate > Keyword: ceramic
3 micrographs available, ordered by micrograph number.
Micrograph
160
:
Glass ceramic, heat treated at 750° C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
162
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
164
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
Help is available on browsing.