Browse the Library
Categories > Ceramic > ZrO2-Y2O3 > Scanning electron microscopy (SEM) > Keyword: zirconia
1 micrograph available, ordered by micrograph number.
Micrograph
849
:
Partially stabilized zirconia (PSZ) powder for plasma spraying System: ZrO2-Y2O3, Composition: ZrO2 92.5, Y2O3 7.5 (wt%) Scanning electron microscopy (SEM) 100 μm |
Help is available on browsing.