Categories > Ceramic > SiC fibre-reinforced magnesium aluminosilicate > Reflected light microscopy > Keyword: porosity
1 micrograph available, ordered by micrograph number.
Micrograph
545
:
Fibre reinforced magnesium aluminosilicate ceramic showing black areas of porosity System: SiC fibre-reinforced magnesium aluminosilicate, Composition: Not specified Reflected light microscopy 100 μm |