Browse the Library
Categories > Ceramic > Soda-lime-silica glaze > Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%) > Keyword: devitrification
2 micrographs available, ordered by micrograph number.
Micrograph
650
:
Small ceramic pot showing centimetre scale crystals within the glaze System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%) Photography (no microscope) 20 mm |
|
Micrograph
655
:
Small ceramic pot showing centimetre scale crystals within the glaze System: Soda-lime-silica glaze, Composition: Soda-lime-silica glaze containing zinc oxide 25, cobalt oxide 0.5 (wt%) Photography (no microscope) 5 mm |