Link to full record for micrograph 148 Micrograph 148 : Magnesia-chrome refractory brick
System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%)
Reflected light microscopy
1 mm
Link to full record for micrograph 149 Micrograph 149 : Magnesia-chrome refractory brick
System: MgO-Cr2O3, Composition: MgO 70, Cr2O3 19, Al2O3 4, Fe2O3 4, CaO 1, SiO2 1 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 150 Micrograph 150 : Alumina-zirconia-silica (AZS) refractory brick
System: Al2O3-ZrO2-SiO2, Composition: Al2O3 50, ZrO2 32, SiO2 15 (wt%), + trace alkalis
Reflected light microscopy
300 μm
Link to full record for micrograph 151 Micrograph 151 : Alumina-graphite brick
System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few%
Reflected light microscopy
400 μm
Link to full record for micrograph 154 Micrograph 154 : Macor(TM) Machinable Glass Ceramic
System: MAS (MgO-Al2O3-SiO2), Composition: SiO2 47, B2O3 8, Al2O3 17, MgO 14, K2O 9, F 6 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 155 Micrograph 155 : Silica investment casting core
System: SiO2, Composition: SiO2, trace of clay
Reflected light microscopy
300 μm