Browse the Library
Categories > Ceramic > Transmitted polarised light microscopy, with sensitive tint plate > Keyword: silica
6 micrographs available, ordered by micrograph number.
Micrograph
172
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
173
:
Bone china, showing the glaze on the surface (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
|
Micrograph
174
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
|
Micrograph
542
:
Devitrified Glass: glass sample heated at 900°C for 17 hours. System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
543
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
|
Micrograph
544
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
Help is available on browsing.