Browse the Library
Categories > Ceramic > Transmitted polarised light microscopy, with sensitive tint plate > Keyword: glass
6 micrographs available, ordered by micrograph number.
Micrograph
160
:
Glass ceramic, heat treated at 750° C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
162
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
164
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
542
:
Devitrified Glass: glass sample heated at 900°C for 17 hours. System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
543
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
|
Micrograph
544
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |