Browse the Library
Categories > Ceramic > Transmitted polarised light microscopy, with sensitive tint plate > Keyword: ceramic
13 micrographs available, ordered by micrograph number.
Showing 11 - 13 of 13 micrographs | Page 1 2 | Previous | Next |
Micrograph
542
:
Devitrified Glass: glass sample heated at 900°C for 17 hours. System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
|
Micrograph
543
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
|
Micrograph
544
:
Devitrified Glass: glass sample heated at 900°C for 17 hours System: SiO2, Composition: Mostly silica, SiO2 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
Showing 11 - 13 of 13 micrographs | Page 1 2 | Previous | Next |