Categories > Composite > Polypropylene with 15% glass fibres > Reflected light microscopy > Keyword: alignment

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 596 Micrograph 596 : Glass-fibre reinforced polymer
System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres
Reflected light microscopy
400 μm