Categories > Composite > Commercial purity (99.5%) + 15 micron angular alumina particles
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
616
:
Cavity formation in a tensile loaded alumina particulate composite System: Al, Composition: Commercial purity (99.5%) + 15 micron angular alumina particles Scanning electron microscopy (SEM) 80 μm |