Categories > Composite > Al2O3, C up to 30 (wt%), Si few% > Reflected light microscopy > Keyword: brick

1 micrograph available, ordered by micrograph number.


Link to full record for micrograph 151 Micrograph 151 : Alumina-graphite brick
System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few%
Reflected light microscopy
400 μm