Browse the Library
Categories > Composite > Keyword: carbon
9 micrographs available, ordered by micrograph number.
Micrograph
151
:
Alumina-graphite brick System: Al2O3-C-Si, Composition: Al2O3, C up to 30 (wt%), Si few% Reflected light microscopy 400 μm |
|
Micrograph
166
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 250 μm |
|
Micrograph
167
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 100 μm |
|
Micrograph
168
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 250 μm |
|
Micrograph
169
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 40 μm |
|
Micrograph
193
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |
|
Micrograph
194
:
MgO-C Refractory Brick System: MgO-C, Composition: MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition Reflected light microscopy 200 μm |
|
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
|
Micrograph
619
:
Tensile failure surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.