Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Composite
24 compositions available. The number of micrographs available is given in [brackets].
- Aggregate, cement, water [2]
- Show relevant: techniques, keywords, micrographs
- Al, Mg 2.5 (wt%), with Al2O3 (10 vol%) [1]
- Show relevant: techniques, keywords, micrographs
- Al, Mg 2.5 (wt%), with Al2O3 (5 vol%) [1]
- Show relevant: techniques, keywords, micrographs
- Al2O3, C up to 30 (wt%), Si few% [1]
- Show relevant: techniques, keywords, micrographs
- Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' [2]
- Show relevant: techniques, keywords, micrographs
- Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle' [1]
- Show relevant: techniques, keywords, micrographs
- Carbon fibre, epoxy resin matrix [2]
- Show relevant: techniques, keywords, micrographs
- Commercial purity (99.5%) [1]
- Show relevant: techniques, keywords, micrographs
- Commercial purity (99.5%) + 13 micron alumina spheroids [1]
- Show relevant: techniques, keywords, micrographs
- Commercial purity (99.5%) + 15 micron angular alumina particles [1]
- Show relevant: techniques, keywords, micrographs
- Commercial purity (99.5%) + 15 micron angular silicon carbide particles [1]
- Show relevant: techniques, keywords, micrographs
- Expanded vermiculite, cured in ZnO and mixed with binder [2]
- Show relevant: techniques, keywords, micrographs
- Kevlar fibre, epoxy resin matrix [3]
- Show relevant: techniques, keywords, micrographs
- Mg 94.05, Zn 5.62, Zr 0.19, Ce 0.10, Nd 0.03 (wt%) (RZ5 Alloy), reinforced with Alumina fibres with a volume fraction of 14% [1]
- Show relevant: techniques, keywords, micrographs
- MgO 50-90, C 8-37 (wt%), remainder Al, Si metal addition [2]
- Show relevant: techniques, keywords, micrographs
- Not specified (System: Glass fibre composite) [2]
- Show relevant: techniques, keywords, micrographs
- Not specified (System: CCcomposite) [11]
- Show relevant: techniques, keywords, micrographs
- Not specified (System: Si3N4-SiC composite) [6]
- Show relevant: techniques, keywords, micrographs
- Not specified (System: Polyurethane (PU)) [4]
- Show relevant: techniques, keywords, micrographs
- Polypropylene matrix with glass fibre [2]
- Show relevant: techniques, keywords, micrographs
- Polypropylene with 15% glass fibres [1]
- Show relevant: techniques, keywords, micrographs
- PS - 15%PB [1]
- Show relevant: techniques, keywords, micrographs
- PS - 35%PB [1]
- Show relevant: techniques, keywords, micrographs
- ZrO2 5-30, Al2O3 70-95 (wt%) [1]
- Show relevant: techniques, keywords, micrographs
Help is available on browsing.