Micrograph
557
:
High Impact Polystyrene (HIPS) System: High Impact Polystyrene (HIPS), Composition: PS - 15%PB Transmitted light microscopy 10 μm |
![]() |
Micrograph
558
:
High Impact Polystyrene (HIPS) System: High Impact Polystyrene (HIPS), Composition: PS - 35%PB Transmitted light microscopy 20 μm |
![]() |
Micrograph
579
:
SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 800 μm |
![]() |
Micrograph
580
:
High magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 160 μm |
![]() |
Micrograph
581
:
X-ray tomography image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified X-ray tomography 1.5 mm |
![]() |
Micrograph
582
:
Low magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 4 mm |
![]() |
Micrograph
596
:
Glass-fibre reinforced polymer System: Polypropylene (PP), Composition: Polypropylene with 15% glass fibres Reflected light microscopy 400 μm |
![]() |
Micrograph
597
:
Frozen stress photoelastic fringe pattern during fibre pushout System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
598
:
Frozen stress photoelastic assessment of load distribution around a cylinder System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
![]() |
Micrograph
599
:
Frozen stress photoelastic assessment of load distribution around an ellipsoid System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle' Cross-polarised light microscopy 6 mm |