Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Composite > CCcomposite
13 micrographs available, ordered by micrograph number.
| Showing 1 - 10 of 13 micrographs | Page 1 2 | Previous | Next |
![]() |
Micrograph
131
:
Unidirectional T800 carbon fibres in an MTM49 epoxy matrix. System: CCcomposite, Composition: Not specified Reflected light microscopy 250 μm |
![]() |
Micrograph
132
:
Woven T800 carbon fibres in an MTM49 epoxy matrix. System: CCcomposite, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
166
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 250 μm |
![]() |
Micrograph
167
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
168
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 250 μm |
![]() |
Micrograph
169
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 40 μm |
![]() |
Micrograph
618
:
Fracture surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 600 μm |
![]() |
Micrograph
619
:
Tensile failure surface of a carbon fibre composite System: CCcomposite, Composition: Carbon fibre, epoxy resin matrix Scanning electron microscopy (SEM) 100 μm |
![]() |
Micrograph
670
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 400 μm |
![]() |
Micrograph
671
:
Carbon-carbon composite System: CCcomposite, Composition: Not specified Reflected light microscopy 200 μm |
| Showing 1 - 10 of 13 micrographs | Page 1 2 | Previous | Next |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.