Browse the Library
Categories > Composite > High Impact Polystyrene (HIPS) > Transmitted light microscopy > Keyword: composite material
2 micrographs available, ordered by micrograph number.
Micrograph
557
:
High Impact Polystyrene (HIPS) System: High Impact Polystyrene (HIPS), Composition: PS - 15%PB Transmitted light microscopy 10 μm |
|
Micrograph
558
:
High Impact Polystyrene (HIPS) System: High Impact Polystyrene (HIPS), Composition: PS - 35%PB Transmitted light microscopy 20 μm |