Browse the Library
Categories > Polymer > Liquid crystalline polymer > Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1) > Cross-polarised light microscopy > Keyword: polymer
2 micrographs available, ordered by micrograph number.
Micrograph
566
:
Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1) Cross-polarised light microscopy 50 μm |
|
Micrograph
567
:
Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1) Cross-polarised light microscopy 50 μm |