Categories > Polymer > Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1) > Cross-polarised light microscopy > Keyword: nematic

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 566 Micrograph 566 : Inversion wall revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm
Link to full record for micrograph 567 Micrograph 567 : Wedge disclinations revealed by spontaneous band texture in a liquid crystalline polymer
System: Liquid crystalline polymer, Composition: Rigid copolyester of hydroxybenzoate (HBA) and hydroxynapthoate (HNA) (1:1)
Cross-polarised light microscopy
50 μm