Browse the Library
Categories > Polymer > Not specified (Polyethylene terephthalate (PET)) > Cross-polarised light microscopy > Keyword: polyethylene terephthalate (PET)
1 micrograph available, ordered by micrograph number.
Micrograph
568
:
Strain induced birefringence in a thermoformed PET cup System: Polyethylene terephthalate (PET), Composition: Not specified Cross-polarised light microscopy 8 mm |