Categories > Polymer > Random copolyester of average molecular weight 14402
1 micrograph available, ordered by micrograph number.
![]() |
Micrograph
642
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402 Scanning electron microscopy (SEM) 12 μm |