Browse the Library

Categories > Polymer > Not specified > Keyword: tissue engineering

4 micrographs available, ordered by micrograph number.


Link to full record for micrograph 114 Micrograph 114 : Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 350-550 micrometre, porosity estimated at 35-45%
System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified
Scanning electron microscopy (SEM)
3 mm
Link to full record for micrograph 115 Micrograph 115 : Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 350-550 micrometre, porosity estimated at 35-45%
System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified
Scanning electron microscopy (SEM)
250 μm
Link to full record for micrograph 116 Micrograph 116 : Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Enlargement of a Pore. Average Pore Size 350-550 mm, porosity estimated at 35-45%
System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified
Scanning electron microscopy (SEM)
250 μm
Link to full record for micrograph 118 Micrograph 118 : Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 100-300 µm, porosity estimated at 65%
System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified
Scanning electron microscopy, environmental
400 μm