Micrograph
642
:
Fracture surface in a liquid crystalline polymer System: Liquid crystalline polymer, Composition: Random copolyester of average molecular weight 14402 Scanning electron microscopy (SEM) 12 μm |
|
Micrograph
643
:
Aligned carbon nanotubes, coated with a conducting polymer System: Carbon nanotube, Composition: Coating of polypyrrole Scanning electron microscopy (SEM) 1 μm |