Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Browse the Library
Categories > Polymer > Keyword: polyethylene (PE)
6 micrographs available, ordered by micrograph number.
![]() |
Micrograph
555
:
Banded spherulites in a blend of polyethtylenes System: Polyethylene (PE), Composition: LPE:BPE 1:3 Transmission electron microscopy (TEM) 200 nm |
![]() |
Micrograph
556
:
Sheaf-like arrangement of lamellae in a blend of polyethylenes System: Polyethylene (PE), Composition: LPE:BPE 3:1 Transmission electron microscopy (TEM) 200 nm |
![]() |
Micrograph
573
:
Birefringence in a film of polyethylene System: Low density polyethylene (LDPE), Composition: Not specified Cross-polarised light microscopy 14 mm |
![]() |
Micrograph
584
:
External surface of blow-moulded HDPE System: High density polyethylene (HDPE), Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
![]() |
Micrograph
585
:
Internal surface of blow-moulded HDPE System: High density polyethylene (HDPE), Composition: Not specified Scanning electron microscopy (SEM) 6 μm |
![]() |
Micrograph
625
:
Series of laser welds in amorphous PET System: Polyethylene terephthalate (PET), Composition: Amorphous polyethylene terephthalate (APET) Cross-polarised light microscopy 12 mm |
Help is available on browsing.
Alternatively, search the Library (from top right on any page), or use advanced search.