Categories > Polymer > Keyword: polystyrene (PS)
11 micrographs available, ordered by micrograph number.
Showing 11 of 11 micrographs | Page 1 2 | Previous | Next |
Micrograph
589
:
Remnants of crazes on a polystyrene fracture surface System: Polystyrene (PS), Composition: Not specified Scanning electron microscopy (SEM) 8 μm |