| Showing 1 - 10 of 31 micrographs | Page 1 2 3 4 | Previous | Next |
![]() |
Micrograph
114
:
Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 350-550 micrometre, porosity estimated at 35-45% System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified Scanning electron microscopy (SEM) 3 mm |
![]() |
Micrograph
115
:
Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 350-550 micrometre, porosity estimated at 35-45% System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified Scanning electron microscopy (SEM) 250 μm |
![]() |
Micrograph
116
:
Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Enlargement of a Pore. Average Pore Size 350-550 mm, porosity estimated at 35-45% System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified Scanning electron microscopy (SEM) 250 μm |
![]() |
Micrograph
559
:
Shear bands in stressed polycarbonate System: Polycarbonate (PC), Composition: Not specified Scanning electron microscopy (SEM) 800 μm |
![]() |
Micrograph
564
:
Aligned array of nanotubes System: Carbon nanotube, Composition: Not specified Scanning electron microscopy (SEM) 25 μm |
![]() |
Micrograph
565
:
Vapour-grown carbon nanotubes System: Carbon nanotube, Composition: Not specified Scanning electron microscopy (SEM) 5 μm |
![]() |
Micrograph
579
:
SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 800 μm |
![]() |
Micrograph
580
:
High magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 160 μm |
![]() |
Micrograph
582
:
Low magnification SEM image of open cell polyurethane foam System: Polyurethane (PU), Composition: Not specified Scanning electron microscopy (SEM) 4 mm |
![]() |
Micrograph
583
:
SEM image of Velcro (TM) System: Nylon, Composition: Not specified Scanning electron microscopy (SEM) 400 μm |
| Showing 1 - 10 of 31 micrographs | Page 1 2 3 4 | Previous | Next |