Poly (lactic-co-glycolic acid) (PLGA) porous scaffold for tissue engineering. Average Pore Size 100-300 µm, porosity estimated at 65% System: Poly (lactic-co-glycolic acid) (PLGA), Composition: Not specified Scanning electron microscopy, environmental 400 μm |