Categories > Polymer > High density polyethylene (HDPE) > Not specified > Keyword: bottle

2 micrographs available, ordered by micrograph number.


Link to full record for micrograph 584 Micrograph 584 : External surface of blow-moulded HDPE
System: High density polyethylene (HDPE), Composition: Not specified
Scanning electron microscopy (SEM)
400 μm
Link to full record for micrograph 585 Micrograph 585 : Internal surface of blow-moulded HDPE
System: High density polyethylene (HDPE), Composition: Not specified
Scanning electron microscopy (SEM)
6 μm