Browse the Library
Categories > Polymer > Cross-polarised light microscopy > Keyword: shear
4 micrographs available, ordered by micrograph number.
Micrograph
597
:
Frozen stress photoelastic fringe pattern during fibre pushout System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
|
Micrograph
598
:
Frozen stress photoelastic assessment of load distribution around a cylinder System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with cylindrical CT200/HT901 'fibre' Cross-polarised light microscopy 6 mm |
|
Micrograph
599
:
Frozen stress photoelastic assessment of load distribution around an ellipsoid System: Araldite (TM), Composition: Araldite CT200/HT907 'matrix' with ellipsoid CT200/HT901 'particle' Cross-polarised light microscopy 6 mm |
|
Micrograph
639
:
Twist-escaped loops in the liquid crystalline polymer MBBA System: Liquid crystalline polymer, Composition: MBBA Cross-polarised light microscopy 200 μm |
Help is available on browsing.