Dissemination of IT for the Promotion of Materials Science (DoITPoMS)

Category

708 micrographs for category Metal or alloy:


Showing 241 - 250 of 708 micrographs Page 1 .. 22 23 24 25 26 27 28 .. 71 | Previous | Next

Link to full record for micrograph 352 Micrograph 352 : Fe, C 0.15 (wt%) steel, quenched.
System: Fe-C-X, Composition: Fe, C 0.15 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 353 Micrograph 353 : Pearlitic malleable cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
800 μm
Link to full record for micrograph 354 Micrograph 354 : Pearlitic malleable cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
400 μm
Link to full record for micrograph 355 Micrograph 355 : Pearlitic malleable cast iron
System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron)
Reflected light microscopy
200 μm
Link to full record for micrograph 356 Micrograph 356 : Pearlitic malleable cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 357 Micrograph 357 : Pearlitic malleable cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 358 Micrograph 358 : White cast iron, annealed to precipitate out carbon
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 359 Micrograph 359 : White cast iron, annealed to precipitate out carbon
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 360 Micrograph 360 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 361 Micrograph 361 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
100 μm

Showing 241 - 250 of 708 micrographs Page 1 .. 22 23 24 25 26 27 28 .. 71 | Previous | Next

List all categories