Link to full record for micrograph 362 Micrograph 362 : White cast iron, subject to slow heating and cooling treatment
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 363 Micrograph 363 : White cast iron, subject to slow heating and cooling treatment
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 364 Micrograph 364 : White cast iron, subject to slow heating and cooling treatment
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 365 Micrograph 365 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ...
Reflected light microscopy
200 μm
Link to full record for micrograph 366 Micrograph 366 : Whiteheart cast iron
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ...
Reflected light microscopy
400 μm
Link to full record for micrograph 367 Micrograph 367 : Whiteheart cast iron
System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), + ...
Reflected light microscopy
200 μm
Link to full record for micrograph 368 Micrograph 368 : Blackheart cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 369 Micrograph 369 : Blackheart cast iron
System: Fe-C-X, Composition: Fe, C 2.4, Si 1.1, Mn 1.1 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 370 Micrograph 370 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 371 Micrograph 371 : As cast white cast iron
System: Fe-C-X, Composition: Fe, C 2.85, Si 0.33, Mn 0.39, Cr 0.91 (wt%)
Reflected light microscopy
100 μm