Category
708 micrographs for category Metal or alloy:
| Showing 321 - 330 of 708 micrographs | Page 1 .. 30 31 32 33 34 35 36 .. 71 | Previous | Next |
![]() |
Micrograph
432
:
Cu 80, Zn 20 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
433
:
Cu 90, Zn 10 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 90, Zn 10 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
434
:
Cu 90, Zn 10 (wt%), recrystallised - annealing twins System: Cu-Zn, Composition: Cu 90, Zn 10 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
435
:
Tough pitch' nearly pure copper, with oxygen impurity System: Cu, Composition: Cu 99.7 (wt%), some oxygen Reflected light microscopy 400 μm |
![]() |
Micrograph
436
:
Tough pitch' nearly pure copper, with oxygen impurity System: Cu, Composition: Cu 99.7 (wt%), some oxygen Reflected light microscopy 200 μm |
![]() |
Micrograph
437
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
438
:
Cu, Sn 20 (wt%) bronze, exhibiting dendritic solidification System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
439
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 800 μm |
![]() |
Micrograph
440
:
a b nickel brass containing 2% lead. System: Cu-Zn, Composition: Cu 46, Zn 42, Ni 10, Pb 2 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
441
:
Cu 60, Zn 40 (wt%) brass, Widmanstätten microstructure System: Cu-Zn, Composition: Cu 60, Zn 40 (wt%) Reflected light microscopy 400 μm |
| Showing 321 - 330 of 708 micrographs | Page 1 .. 30 31 32 33 34 35 36 .. 71 | Previous | Next |