708 micrographs for category Metal or alloy:


Showing 361 - 370 of 708 micrographs Page 1 .. 34 35 36 37 38 39 40 .. 71 | Previous | Next

Link to full record for micrograph 479 Micrograph 479 : Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification
System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 480 Micrograph 480 : Cu 80, Zn 20 (wt%) brass, exhibiting dendritic solidification
System: Cu-Zn, Composition: Cu 80, Zn 20 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 481 Micrograph 481 : Cu 80, Sn 20 (wt%) bronze, as cast
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 482 Micrograph 482 : Cu 80, Sn 20 (wt%) bronze, as cast
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 483 Micrograph 483 : Cu 80, Sn 20 (wt%) bronze, as cast
System: Cu-Sn, Composition: Cu 80, Sn 20 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 484 Micrograph 484 : Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 485 Micrograph 485 : Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 486 Micrograph 486 : Cu 80, Sn 20 (wt%) bronze, exhibiting dendritic solidification
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 487 Micrograph 487 : Cu 85, Sn 15 (wt%) bronze, annealed at 650°C
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
800 μm
Link to full record for micrograph 488 Micrograph 488 : Cu 85, Sn 15 (wt%) bronze, annealed at 650°C
System: Cu-Sn, Composition: Cu 85, Sn 15 (wt%)
Reflected light microscopy
400 μm