708 micrographs for category Metal or alloy:


Showing 451 - 460 of 708 micrographs Page 1 .. 43 44 45 46 47 48 49 .. 71 | Previous | Next

Link to full record for micrograph 697 Micrograph 697 : Cu-4.5 wt% P
System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 698 Micrograph 698 : Cu-4.5 wt% P
System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 699 Micrograph 699 : Cu-4.5 wt% P
System: Cu-P, Composition: Cu 95.5, P 4.5 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 700 Micrograph 700 : Cu-10.5 wt% P
System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%)
Reflected light microscopy
400 μm
Link to full record for micrograph 701 Micrograph 701 : Cu-10.5 wt% P
System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%)
Reflected light microscopy
200 μm
Link to full record for micrograph 702 Micrograph 702 : Cu-10.5 wt% P
System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%)
Reflected light microscopy
100 μm
Link to full record for micrograph 703 Micrograph 703 : Cu-10.5 wt% P
System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%)
Reflected light microscopy
50 μm
Link to full record for micrograph 704 Micrograph 704 : Cu-10.5 wt% P
System: Cu-P, Composition: Cu 89.5, P 10.5 (wt%)
Reflected light microscopy
20 μm
Link to full record for micrograph 705 Micrograph 705 : Cu-? wt% P
System: Cu-P, Composition: Not specified
Reflected light microscopy
400 μm
Link to full record for micrograph 706 Micrograph 706 : Cu-? wt% P
System: Cu-P, Composition: Not specified
Reflected light microscopy
200 μm