Micrograph
717
:
IN718 nickel-based superalloy held for 6 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
718
:
IN718 nickel-based superalloy held for 24 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
719
:
IN718 nickel-based superalloy held for 48 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
720
:
IN718 nickel-based superalloy held for 72 hours at 850°C System: Ni-X, Composition: Ni 53, Fe 19, Cr 18, Nb 5 (wt% approx) + small amounts of Ti, Mo, Co, Al Reflected light microscopy, cross-polarised, with Nomarski filter 25 μm |
![]() |
Micrograph
721
:
Ni-Superalloy System: Ni-X, Composition: Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy) Field emission gun scanning electron microscopy (FEGSEM) in secondary electron imaging (SEI) mode 10 μm |
![]() |
Micrograph
722
:
Ni-Superalloy System: Ni-X, Composition: Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy) Field emission gun scanning electron microscopy (FEGSEM) in secondary electron imaging (SEI) mode 6 μm |
![]() |
Micrograph
723
:
Ni-Superalloy System: Ni-X, Composition: Ni, Al, Re, W, Ta, Cr, Co, Ru (Ni-Superalloy) Transmission electron microscopy (TEM) 200 nm |
![]() |
Micrograph
724
:
Ni-Superalloy, as-extruded microstructure System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
725
:
Ni-Superalloy, as-extruded microstructure System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |
![]() |
Micrograph
726
:
Ni-Superalloy, heat treated above gamma-prime solvus System: Ni-X, Composition: Ni, Cr 14.4-15.2, Co 13-18, Mo 3.5-4.5, Al 3.0-3.3, Ti 4.2-4.8, Ta 2.5, Zr 0.05-0.07, C 0.05, B 0.01-0.03 (wt%) (Ni-Superalloy) Scanning electron microscopy (SEM) in backscattered electron imaging (BEI) mode 10 μm |