Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Category
708 micrographs for category Metal or alloy:
| Showing 531 - 540 of 708 micrographs | Page 1 .. 51 52 53 54 55 56 57 .. 71 | Previous | Next |
![]() |
Micrograph
780
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
781
:
Heat treated spheroidal graphite cast iron System: Fe-C-X, Composition: Fe, C 3.2, Si 2.5, Mg 0.05 (wt%) Reflected light microscopy 50 μm |
![]() |
Micrograph
782
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
783
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
784
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
785
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
786
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
787
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 20 μm |
![]() |
Micrograph
788
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
789
:
Austempered ductile cast iron System: Fe-C-X, Composition: Fe, C 3.52, Si 2.51, Mn 0.49, Mo 0.15, Cu 0.31 (wt%) Reflected light microscopy 40 μm |
| Showing 531 - 540 of 708 micrographs | Page 1 .. 51 52 53 54 55 56 57 .. 71 | Previous | Next |