708 micrographs for category Metal or alloy:
| Showing 561 - 570 of 708 micrographs | Page 1 .. 54 55 56 57 58 59 60 .. 71 | Previous | Next |
![]() |
Micrograph
810
:
Ferritic steel heat treated and water quenched System: Fe-C-X, Composition: Fe, Mn 1, S 0.02 (wt%) Scanning electron microscopy (SEM) 1.5 μm |
![]() |
Micrograph
811
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
812
:
Austenitic stainless steel rapidly cooled, fracture surface of laboratory ingot System: Fe-C-X, Composition: Fe, C 0.13, Ni 4, Cr 2, Mn 0.49, S 0.015 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
813
:
Austenitic stainless steel solution treated, quenched and tempered, with M23C6 precipitate System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
![]() |
Micrograph
814
:
Austenitic stainless steel solution treated, quenched and tempered System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Nb 1 (wt%) Transmission electron microscopy (TEM) 1 μm |
![]() |
Micrograph
815
:
Martensitic steel, lightly rolled, with dislocations in austenite System: Fe-C-X, Composition: Fe, C 0.2, Mo 4 (wt%) Scanning electron microscopy (SEM) 400 nm |
![]() |
Micrograph
816
:
Austenitic stainless steel solution treated, quenched and tempered, showing M23C6 precipitate System: Fe-C-X, Composition: Stainless steel with Cr 18, Ni 10, Mo 1 (wt%) Transmission electron microscopy (TEM) 400 nm |
![]() |
Micrograph
817
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Ti 5, C 0.1 Scanning electron microscopy (SEM) 2 μm |
![]() |
Micrograph
818
:
Austenitic stainless steel tempered System: Fe-C-X, Composition: Stainless steel with Cr 15, Ni 35, Nb 2.5, C 0.1 (wt%) Scanning electron microscopy (SEM) 4 μm |
![]() |
Micrograph
819
:
Austenitic stainless steel water quenched then deformed in impact System: Fe-C-X, Composition: Stainless steel with Cr 13.7, Mn 14.2, C 0.12 (wt%) Reflected light microscopy 50 μm |