Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Category
708 micrographs for category Metal or alloy:
| Showing 611 - 620 of 708 micrographs | Page 1 .. 59 60 61 62 63 64 65 .. 71 | Previous | Next |
![]() |
Micrograph
878
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
879
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag System: Smithing slag, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
880
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
881
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Reflected light microscopy 200 μm |
![]() |
Micrograph
882
:
Nörten-Hardenberg (Goettingen) Germany. Smithing slag (hallstatt - latène) System: Smithing slag, Composition: Not specified Transmitted light microscopy 200 μm |
![]() |
Micrograph
883
:
Hambach forest, Germany. Medieval smithing slag System: Smithing slag, Composition: Not specified Reflected light microscopy 100 μm |
![]() |
Micrograph
884
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silverproduction from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
885
:
Monte Romero, Huelva district, Spain. Phoenician, preroman silver production from complex ores. System: Pre-Roman Ag production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
886
:
Maroni, Cyprus, copper slag System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
![]() |
Micrograph
887
:
Maroni, Cyprus, copper slag System: Cu production, Composition: Not specified Reflected light microscopy 500 μm |
| Showing 611 - 620 of 708 micrographs | Page 1 .. 59 60 61 62 63 64 65 .. 71 | Previous | Next |