92 micrographs for category Ceramic:
| Showing 11 - 20 of 92 micrographs | Page 1 2 3 4 5 6 7 .. 10 | Previous | Next |
![]() |
Micrograph
155
:
Silica investment casting core System: SiO2, Composition: SiO2, trace of clay Reflected light microscopy 300 μm |
![]() |
Micrograph
160
:
Glass ceramic, heat treated at 750° C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
161
:
Glass ceramic, heat treated at 750°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |
![]() |
Micrograph
162
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
163
:
Glass ceramic, heat treated at 840°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |
![]() |
Micrograph
164
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
165
:
Glass ceramic, heat treated at 900°C for 3 hours System: LAS: Li2O-Al2O3-SiO2, Composition: Not specified Transmitted polarised light microscopy 100 μm |
![]() |
Micrograph
170
:
ZnO varistor System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3 Transmitted polarised light microscopy, with sensitive tint plate 100 μm |
![]() |
Micrograph
171
:
ZnO varistor System: ZnO, Composition: ZnO containing small amounts of oxides such as Sb2O3 and Bi2O3 Transmitted polarised light microscopy, with sensitive tint plate 250 μm |
![]() |
Micrograph
172
:
Bone china (with sensitive tint plate) System: Bone china, Composition: China clay 25, stone 30, bone 45 (wt% typical) Transmitted polarised light microscopy, with sensitive tint plate 100 μm |