Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
2 micrographs for composition Al 75, Cu 25 (wt%), ordered by micrograph number.
![]() |
Micrograph
1
:
Al 75, Cu 25 (wt%), hypoeutectic alloy System: Al-Cu, Composition: Al 75, Cu 25 (wt%) Reflected light microscopy 40 μm |
![]() |
Micrograph
2
:
Al 75, Cu 25 (wt%), hypoeutectic alloy System: Al-Cu, Composition: Al 75, Cu 25 (wt%) Scanning electron microscopy (SEM) 30 μm |