Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
7 micrographs for composition Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%), ordered by micrograph number.
![]() |
Micrograph
328
:
Nickel low carbon steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 200 μm |
![]() |
Micrograph
329
:
Nickel low carbon steel, quenched and tempered System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
340
:
Low alloy medium carbon steel, containing Ni, Cr, Mo, annealed System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
341
:
Low alloy medium carbon steel, containing Ni, Cr, Mo, annealed System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
342
:
Medium carbon, low alloy steel System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
343
:
Medium carbon, low alloy steel System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |
![]() |
Micrograph
344
:
Medium carbon, low alloy steel. System: Fe-C-X, Composition: Fe, C 0.31, Ni 3.0, Cr 0.9, Mn 0.6 (wt%) Reflected light microscopy 100 μm |