Composition
25 micrographs for composition Fe, C 2-4, other constituents (wt% typical) (Cast iron), ordered by micrograph number.
| Showing 1 - 10 of 25 micrographs | Page 1 2 3 | Previous | Next |
![]() |
Micrograph
66
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
67
:
Hypoeutectic white cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 80 μm |
![]() |
Micrograph
68
:
Grey cast iron core with white cast iron periphery System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
69
:
Grey cast iron core with white cast iron periphery System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 40 μm |
![]() |
Micrograph
353
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 800 μm |
![]() |
Micrograph
354
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
355
:
Pearlitic malleable cast iron System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
393
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
394
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
395
:
Cast iron with magnesium induced spheroidised graphite System: Fe-C-X, Composition: Fe, C 2-4, other constituents (wt% typical) (Cast iron) Reflected light microscopy 100 μm |