Composition
3 micrographs for composition Fe, C 3.4, Si 0.35, Mn 0.22 (wt%), ordered by micrograph number.
![]() |
Micrograph
362
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
363
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 400 μm |
![]() |
Micrograph
364
:
White cast iron, subject to slow heating and cooling treatment System: Fe-C-X, Composition: Fe, C 3.4, Si 0.35, Mn 0.22 (wt%) Reflected light microscopy 100 μm |