Micrograph Library
Browse the libraryAdvanced searchSystemsCompositionsTechniquesKeywordsPhase diagramsHelpPreferencesAbout the micrograph libraryTerms of useContribute micrographs!FeedbackLinksCredits Print this page

Composition
3 micrographs for composition Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron), ordered by micrograph number.
![]() |
Micrograph
378
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 400 μm |
![]() |
Micrograph
379
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 200 μm |
![]() |
Micrograph
380
:
Grey cast iron with significant Si content System: Fe-C-X, Composition: Fe, C 3.52, Si 3.26, Mn 0.47 (wt%) (Grey cast iron) Reflected light microscopy 100 μm |